Lumut Naval Shipyard · Jabatan ISD — QIR

Borang Pemeriksaan Kualiti

Project Name
Order No.
Material
Heat No.
Edge Preparation
Root Gap
Alignment Hi Low
Alignment Angular
Joint Type
Hi Low Angular
Result
Project Name
Order No.
Welder No.
Welding Process
Butt Joint (Yes/No)
Throat Size (mm)
Intermittent (Yes/No)
Throat Size (mm)
Undercut
Excess Weld Metal
Slag Inclusion
Porosity
LOF/LOP
Crack/Lamination
Others
No Apparent Defect
Result
Project Name
Order No.
Environment Condition
Time
Dry Bulb (°C)
Wet Bulb (°C)
Steel Temperature (°C)
Dew Point (°C)
Relative Humidity (%)
Weather
Surface Preparation
Surface Profile
Surface Cleanliness
Abrasive Type
Inspection Result
No. Of Coat Product Name Batch Number DFT Req. (µm) DFT/Coat (µm) R1 R2 R3 R4 R5 Avg DFT (µm)